He should be it feed straight to the bottom line. A fact that will show up in the PFS.
What's more on the weekend I implied we could beat those recoveries since: - We haven't allowed to the pre-conditioning of water re- cycled from tailings etc. which will allow more time for collector to coat particles durig grinding etc. - We haven't yet properly explored the use of magnetic separation to concentrate the magnetic Ni minerals and PGM's that go with them directing to the optimal point in the circuit. It could be in the middle at regrind or end. Magnetic concentration on the scavengers may also be useful.